International code name
|
SK35 | SK36 | SK37 | SK38 | SK40 |
|
Al2O3/%
|
≥48 | ≥55 | ≥65 | ≥75 | ≥80 |
|
Fe2O3/%
|
≤2 | ≤2 | ≤2 | ≤2 | ≤2 |
|
Refractoriness
|
≥1750 °C | ≥1770 °C | ≥1790 °C | ≥1790 °C | ≥1790 °C |
|
Apparent porosity
|
≤22% | ≤22% | ≤23% | ≤23% | ≤21% |
|
Cold crushing strength
|
≥39Mpa | ≥44Mpa | ≥49Mpa | ≥54Mpa | ≥65Mpa |
|
Refractoriness under load (0.2MPa)
|
≥1420 °C | ≥1470°C | ≥1500 °C | ≥1520 °C | ≥1530 °C |
| Reheating Linear Change (1500°C 2h) % |
+0.1~ -0.4
*1450°C |
+0.1~ -0.4 | +0.1~ -0.4 |
|
+0.1~ -0.4 |