Honeycomb ceramic regeneration have significant advantages such as high temperature resistance, corrosion resistance, good thermal shock stability, high strength, large heat storage capacity, and good thermal conductivity, greatly increasing their effectiveness and service life.
|
Category |
Measurement |
Parameter |
|
|
Cordierite |
% |
≥95 |
|
|
Thermal expansion Coefficient (RT-800ºC) |
m/ºC |
≤1.3×10-6 |
|
|
Thermal shock resistance(RT-550ºC) |
Cycle times |
≥3 |
|
|
Softening temperature |
ºC |
≥1360 |
|
|
Compressive strength |
Parallel direction |
MPa |
≥10 |
|
Vertical direction |
MPa |
≥3 |
|
|
Mesh |
Mesh |
100-600 |
|
|
Water absorption rate |
% |
20-28 |
|
|
Wall thickness |
mm |
0.13-0.23 |
|
|
Tolerance range |
mm |
≤0.8 |
|
|
Item |
Index |
Specifications |
|
Material |
Cordierite |
Round Size:Φ80×12.5mm, Φ100×50mm, Φ125×12.5mm, Φ150×12.5mm, Φ160×13.5mm, Φ168×13.5 mm
|
|
Water absorption |
50.40% |
|
|
Open Porosity |
61% |
|
|
Specific gravity |
0.9-1.10Kg/cm3 |
|
|
Temperature softening |
>1280 °C |
|
|
Cooking Surface Temperature |
1000-1200 |
|
|
CO Release |
≤0.006% |
|
|
NOx Release |
≤5ppm |