| CHEMICAL COMPOSITION | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | V |
| 1.45-1.60 | 0.10-0.60 | 0.20-0.60 | ≤0.030 | ≤0.030 | 11.0-13.0 | / | 0.70-1.00 | 0.70-1.00 |
| PRODUCTION FLOW&TECHNICAL INDEX | |
| Size Range | Round 80-800mm; Flat 80-400mmx300-1000mm |
| Smelting | EAF+LF+VD(or +ESR) |
| Production Process | Hot Forged+Spheriodizing Annealing ≤ 255HB |
| Heat Treatment |
Softening annealing at a temperature of 820 - 860°C.
Relief annealing in the range of 600 - 700°C. Hardening at a temperature of 960 - 1030°C. Tempering in air at a temperature of 220 - 550°C. |
| Forging Ratio | ≥ 6:1 |
| Surface | Machined |
| Non-metallic Inclusions |
Acc. To ASTM E45 or finer
A(Thin 1.0 Heavy 1.0); B(Thin 1.0 Heavy 1.0); C(Thin 1.0 Heavy 1.0); D((Thin 1.0 Heavy 1.0); |
| Grain Size | Acc. To ASTM E112 ≥ 5 or finer |
| UT | SEP1921-84 3 D/d or finer |
| Alloy Steel |
4140,4142,42CrMo4,1.7225,SCM440,4130,SCM430,25CrMo4,1.7218,34CrNiMo6,
1.6582,4340,SNCM439,36CrNiMo4,1.6511,SACN645,1340,SMn438,SNC236, |
| Tool Steel |
H13,1.2344,SKD61,D2,SKD11,1.2379,1.2510,01,SKS3,95MnWCr5,D3,SKD1,1.2419,
SKS31,H21,SKD5,1.2581,P20,35CrMo7,1.2738,1.2316,M2 |
| Bearing Steel | GCr15,52100,SUJ1,SUJ2,100Cr6,1.2067,55C,8620,4320,9310,440C,M50 |
| Spring Steel |
9260,SUP6,SUP7,1.7108,54SiCr6,1.7102,5155,SUP9,1.7176,5160,1.7177,6150,
SUP10,51CrV4,1.8159 |
| Stainless Steel |
321,sus321,1.4541,304,SUS304,1.4301,410,SUS410,1.4006,420,1.4021,1.4028,
434,1.4113,316L,SUS316L,1.4435,630,1.4542,431,1.4057 |